superalloy

 metallurgy

Main

Aspects of this topic are discussed in the following places at Britannica.

Assorted References

  • materials science ( in materials science: Alloying )

    These advances in processing have been accompanied by the development of new “superalloys.” Superalloys are high-strength, often complex alloys that are resistant to high temperatures and severe mechanical stress and that exhibit high surface stability. They are commonly classified into three major categories: nickel-based, cobalt-based, and iron-based. Nickel-based superalloys...

  • use ( in molybdenum processing: Superalloys )

    Nonferrous alloys categorized under the name superalloys or nimonics account for about 3 percent of the total demand for molybdenum. They are used in jet engines, nuclear plants, gas turbines, space exploration, and general aviation.

Citations

MLA Style:

"superalloy." Encyclopædia Britannica. 2009. Encyclopædia Britannica Online. 02 May. 2009 <http://www.britannica.com/EBchecked/topic/574179/superalloy>.

APA Style:

superalloy. (2009). In Encyclopædia Britannica. Retrieved May 02, 2009, from Encyclopædia Britannica Online: http://www.britannica.com/EBchecked/topic/574179/superalloy

TABLE OF CONTENTS

The Britannica Store
A-Z Browse

We welcome your comments. Any revisions or updates suggested for this article will be reviewed by our editorial staff.
Contact us here.

This is a BETA release of TOPIC HISTORY
Type
Title
Description
Contributor
Date
Send
Link to this article and share the full text with the readers of your Web site or blog post.

If you think a reference to this article on "" will enhance your Web site, blog post, or any other Web content, then feel free to link to it, and your readers will gain complete access to the full article, even if they do not subscribe to our service.

You may want to use the HTML code fragment provided below. Copy Link
Enter the e-mail address you used when enrolling for Britannica Premium Service and we will e-mail your password to you.
Did You Mean...
All Results
There are currently no results related to your search. Please check to see that you spelled your query correctly. Or, try a different or more general query term.
Image preview